A nanotecnologia aplicada à prevenção da corrosão : o uso de nanocerâmicos de alumina e zircônia

dataload.collectionmapped02 - Mestrado - Químicapt_BR
dataload.filenamenourau1549.pdfpt_BR
dataload.handlemapped123456789/55pt_BR
dataload.idpergamum135085pt_BR
dataload.idvirtuanourauvtls000146610pt_BR
dataload.idvirtuapergamumvtls000146610pt_BR
dataload.idvirtuapergamum.sameurlnourauSIMpt_BR
dataload.linknourauhttp://www.bibliotecadigital.uel.br/document/?code=vtls000146610pt_BR
dataload.linknourau.regularSIMpt_BR
dataload.linknourau.retificadohttp://www.bibliotecadigital.uel.br/document/?code=vtls000146610pt_BR
dataload.linknourau.size64.00pt_BR
dc.contributor.advisorDall'Antonia, Luiz Henrique [Orientador]pt_BR
dc.contributor.authorSouza Junior, Osmar Batista dept_BR
dc.contributor.bancaGarcia, Jarem Raulpt_BR
dc.contributor.bancaSantana, Henrique dept_BR
dc.coverage.spatialLondrinapt_BR
dc.date.accessioned2024-05-01T13:45:28Z
dc.date.available2024-05-01T13:45:28Z
dc.date.created2008.00pt_BR
dc.date.defesa21.11.2008pt_BR
dc.description.abstractResumo: Este trabalho apresenta o estudo de um material nanocerâmico com matriz de Al2O3 adicionado 15% em mol de ZrO2 como material inibidor de corrosão nos substratos metálicos: aço carbono, aço galvanizado minimizado e alumínio A caracterização dos óxidos formados foi realizada pelo estudo da Espectroscopia no Infravermelho com Transformada de Fourier (FTIR, “Fourier Transfomed Infrared Spectroscopy”) e difração de Raios X A partir dos resultados de difração de Raios X foi possível demonstrar a fase majoritária do óxido formado, bem como cálcular o diâmetro das nanopartículas A eficiência da inibição contra corrosão nos diferentes substratos metálicos foram comparadas a peças pré-tratadas pelos processos de fosfatização convencional e um material nanocerâmico já utilizado na indústria Os ensaios eletroquímicos investigativos quanto a eficiência na inibição da corrosão compreenderam curvas de potencial em função tempo, em circuito aberto, curvas de polarização potenciodinâmica para análise de estabilidade e resistência dos filmes contra corrosão e voltametria cíclica Experimentos de teste de névoa salina (‘salt spray’) com tempo de exposição de 5 horas para verificação do desempenho do compósito Al2O3/ZrO2 contra corrosão, em placas com revestimento orgânico, demonstraram que houve apenas migração de corrosão no corte de 3 a 5 mm para aço carbono e no aço galvanizado ocorreu o processo de corrosão branca do zinco e nenhuma relacionada ao alumínio Os resultados foram bastante satisfatórios e demonstraram que estes materiais sintetizados, a base de nanocerâmicos, podem substituir processos convencionais de fosfatização que são do ponto de vista ambiental muito mais impactantes ao ambientept_BR
dc.description.abstractother1Abstract: This work presents the study of a nanoceramic material, based on a matrix of Al2O3 with addition of ZrO2 15% in mol, as corrosion inhibitor in metallic substrates: steel carbon, steel galvanized minimized and aluminum The characterization of the formed oxides was carried out by the study of Fourier´s Transformed Infrared Spectroscopy (FTIR) and Ray X diffraction From the results of Ray X diffraction it was possible to determine the majority phase of formed oxide, as well calculated the nanoparticles diameter The efficiency of the corrosion inhibition from different metallic substrates were compared to pre-treated pieces by conventional phosphatated methods and a nanoceramic zirconium based material, already utilized in the industry The electrochemical methods to investigate the corrosion inhibition efficiency comprehend: curves of potential versus time, at open circuit, curves of potentialdynamics polarization for analysis of stability and resistance of the film against corrosion and cyclic voltammetry Salt spray test experiments during exposition around 5 hours, for verification of the performance of the composite Al2O3/ZrO2 against corrosion, in plates with organic covering, showed that had barely migration of corrosion in the cut of 3 to 5 mm for steel carbon and in the steel galvanized occurred the white corrosion of zinc and nothing related to the aluminum The results were sufficiently acceptable and showed that these synthesized material, based on nanoceramics, can replace conventional phosphatated process, that are more devastating in an environmental perspectivept_BR
dc.description.notesDissertação (Mestrado em Química dos Recursos Naturais) - Universidade Estadual de Londrina, Centro de Ciências Exatas, Programa de Pós-Graduação em Química dos Recursos Naturaispt_BR
dc.identifier.urihttps://repositorio.uel.br/handle/123456789/11817
dc.languagepor
dc.relation.coursedegreeMestradopt_BR
dc.relation.coursenameQuímica dos Recursos Naturaispt_BR
dc.relation.departamentCentro de Ciências Exataspt_BR
dc.relation.ppgnamePrograma de Pós-Graduação em Química dos Recursos Naturaispt_BR
dc.subjectCorrosãopt_BR
dc.subjectPrevençãopt_BR
dc.subjectÓxido de zircôniapt_BR
dc.subjectNanotecnologiapt_BR
dc.subjectAluminapt_BR
dc.subjectCorrosion - Prevention - Nanotechnologypt_BR
dc.titleA nanotecnologia aplicada à prevenção da corrosão : o uso de nanocerâmicos de alumina e zircôniapt_BR
dc.typeDissertaçãopt_BR

Arquivos

Pacote Original
Agora exibindo 1 - 1 de 1
Carregando...
Imagem de Miniatura
Nome:
1549.pdf
Tamanho:
465.89 KB
Formato:
Adobe Portable Document Format